The 18 questions most frequently asked by technical and procurement personnel, organized into four groups: technology and model selection, sample lead times, technical documentation, and commercial compliance. Answers should provide specific figures and troubleshooting sequences wherever possible, rather than saying “it depends.”

FAQ Technical and Selection Q&A
What is the difference between the 30μm and 100μm pore sizes of a PVA brush roller?
Small apertures mean more openings per unit area and stronger capillary capture of submicron particles, but they are more prone to clogging with grinding debris and slurry, resulting in shorter maintenance intervals; large apertures provide better drainage and clogging resistance. A common practice is to use smaller apertures in the post-CMP final cleaning section (30–60 μm) and larger apertures in front-end coarse cleaning and thinning sections. When selecting an aperture, compare samples with two different apertures at the same brush position using particle counts rather than relying only on the parameter sheet.
What usually causes regular arc-shaped scratches on wafers after cleaning with a brush roller?
Check three areas in sequence: first, uneven flash or nodule height on the end face may concentrate contact pressure along an arc; second, excessive shaft-end runout may cause periodic contact as the brush rotates; third, compression may drift after the roller is replaced. The response is to recheck end-face flatness and runout, change to a nodule type if necessary to reduce contact concentration, and reconfirm compression using test wafers.
Where does particle shedding from brushes generally originate?
The three most common sources are low-molecular-weight residue extractables, cutting-end machining residue that has not undergone cleaning, and material introduced through packaging and handling. Corresponding actions are to switch to a low-extractables formulation, ultrasonically clean the end faces, and package each brush individually in a clean bag; water absorption and appearance reinspection records can be provided for production batches.
How often should brush rollers be replaced? Is there a standard calendar interval?
There is no universal calendar interval. The replacement criteria should be based on three curves established for each brush position: the decline in particle removal rate relative to the baseline, water absorption retest results, and end-face runout and appearance. Establish a baseline during the sample stage, then conduct sampling inspections by batch and use the data to determine the replacement point, avoiding both premature scrapping and waiting until batch-level scratching occurs.
Why does compression drift, and how is it detected?
Drift generally comes from three sources: accumulated brush roller outer-diameter tolerance, changes in end-face runout, and axial position shifts after installation. Detection should rely on data rather than feel: record the measured outer diameter after each roller replacement and the first-piece cleaning result, and trend particle counts against compression. When the same model produces different results, first investigate these three items.
What is the difference in resistance between conductive and antistatic filaments?
Conductive filaments are used to rapidly carry charge away. The range commonly used at our site is 10³–10⁶ Ω. They are graded by formulation, and the actual grade shall be based on the measured resistance of the sample piece, and they must be paired with reliable grounding; antistatic filaments have higher resistance, typically 10⁶–10⁹ Ω, and serve to slowly dissipate charge and prevent accumulation. When selecting a grade, first determine whether the operating condition calls for “charge dissipation” or “accumulation prevention,” and then select the grade.
FAQ Prototyping and Lead Time
How long does prototyping take, and is it charged?
For standard structures, the sample lead time is confirmed according to the drawings; complex structures requiring new tooling or special processes are discussed separately. Prototyping is generally charged per piece, and the cost can be credited against the bulk order after the samples pass. Details are provided in the quotation.
What is the minimum order quantity?
Products in the standard range can be ordered by the piece; non-standard items are evaluated based on tooling and process requirements. We support small trial orders, which can be converted to production orders after validation.
How is the lead time for bulk orders calculated?
Typically 2–4 weeks, depending on order volume and production scheduling. Orders requiring custom tooling or special material procurement take longer; the quotation will provide a lead-time range.
Can you expedite orders?
Subject to production scheduling, an order can be submitted for insertion into the schedule, with the impact on other orders evaluated. Expediting is subject to written confirmation; no verbal commitments are made.
FAQ Technical and Documentation
Can you provide specification sheets, RoHS, and MSDS?
Yes. Individual specification sheets are available on request; RoHS and MSDS are provided by batch and in accordance with the customer-specified standards. Please specify the required documents when requesting a quotation.
Can you provide sample test data?
During the sample stage, we can support comparative testing of soak-solution TOC, particle counts, or specified metal ions. The test items and submission method will be confirmed when requesting a quotation.
What is the smallest aperture or finest filament you can supply?
PVA apertures commonly range from 30–100 μm; filament material is available down to 0.05 mm. Extreme specifications require a process-feasibility review and should not be included in drawings before validation.
How are custom parts developed?
Drawings, samples, or a description of the operating conditions are all acceptable. We will first conduct a drawing review to confirm the mounting interface, interference/compression, cleaning objectives, and operating environment, and then produce samples.
FAQ Commercial and Compliance
Can you sign a confidentiality agreement?
Yes. For OEM and non-standard projects, signing an NDA before technical document exchange is recommended, with production and documentation isolated by project.
What are the payment terms and credit period?
These are agreed based on the cooperation stage and order size. The standard terms are advance payment plus settlement before shipment; credit periods may be requested for long-term customers.
Can you accommodate a factory audit?
Yes. We recommend arranging the audit during the technical review stage before a bulk order. Please make an appointment in advance, and we will prepare the relevant documentation and retained samples according to your areas of interest.
How are quality disputes handled?
Batch-retained samples and inspection records are used jointly to confirm the facts. If the issue is confirmed to be on our side, it will be handled as agreed in the contract; where on-site analysis is required, an engineer can be assigned to assist.
Not covered Can't find your question?
The Q&A on the page covers general questions. Judgments involving specific operating conditions, such as tool model, cleaning-fluid system, and acceptance criteria, are best discussed directly, as these are difficult to answer with general information, and any generic answer may not apply.
Customer requirements
Leave your contact details and requirements so we can get in touch.