Case / Advanced Packaging Factory IC Substrate Deburring

Why does FC-BGA substrate burr height keep drifting

Burr height at the cut edge of the substrate was unstable, causing intermittent placement offsets. The problem lay not in abrasive grit size, but in matching the compression to the board-edge profile.

  • FC-BGA substrate
  • Deburring
  • Abrasive filament
  • Delivered 2025
Process floor

Problem Problem

Burr height fluctuated between 20–45 μm, exceeding the ±25 μm control line;

The brush roll was a general-purpose flat roll, resulting in uneven contact between the brush surface and the board-edge profile and excessive compression at the corners.

Solution Approach

  1. Changed to nylon 612 abrasive filament with a helical-wound structure, allowing the brush surface to conform to the board-edge profile;
  2. Chamfered the end face according to the board-edge profile to prevent secondary scratching by end-face flash;
  3. Back-calculated the compression based on line speed and included the compression in the work instruction.

Result Results

≤ 25 μmBurr height
-71%Placement offset defects
+35%Brush roll service life
MetricBefore retrofitAfter retrofit
Burr height20–45 μm≤ 25 μm
Placement offset defectsBaseline 100Baseline 29
Brush roll replacement frequency2 per month1.3 per month

Note Description

“Parameters are not guessed; they are calculated from the board-edge profile.” — Customer Equipment Engineer

The case data follows the de-identified scope of the customer's acceptance records; customer names are withheld for confidentiality, and specific test conditions and acceptance criteria can be provided with factory-audit documentation.

Related Related products and materials

Customer requirements

Leave your contact details and requirements so we can get in touch.

Operating conditions and dimensions

Optional. Saved details are included with your inquiry.