Periodic rebound in particle count is not a sign that the brush roll has reached the end of its service life
Post-wash particle counts rebounded approximately every three weeks and returned to normal after replacing the brush roll—a phenomenon judged on-site to mean that the “brush roll had reached the end of its service life.” We compared three months of roll-replacement records with particle counts and found that the roll-replacement timing did not align with the particle rebound.

Problem Problem
Particle counts began rising in weeks 2–3 after roll replacement and triggered an alarm in week 4, even though the brush roll appeared intact, with no particle shedding or scratches.
The on-site replacement criterion was a “30-day calendar interval,” but the actual pore-clogging rate varied with product structure; the service life of the same brush roll differed twofold across different products.
Solution Approach
- Changed to a low-extractables formulation to reduce secondary pore clogging caused by low-molecular-weight residues;
- Established water-absorption and particle-removal baselines for each brush position, changing the replacement criterion from a calendar interval to data thresholds;
- Used end-face ultrasonic cleaning and clean-bag packaging for each brush to eliminate particle sources introduced by packaging.
Result Results
| Metric | Before retrofit | After retrofit |
|---|---|---|
| Replacement criterion | Fixed 30 days | Dual thresholds: particle baseline + water absorption |
| Particle rebound amplitude | Baseline 100 | Baseline 38 |
| Single-brush cycle | 30 days | 52 days |
Note Description
“Previously, we waited for the alarm before replacing it; now, we know a week in advance that it needs replacing.” — Customer Process Engineer
The case data follows the de-identified scope of the customer's acceptance records; customer names are withheld for confidentiality, and specific test conditions and acceptance criteria can be provided with factory-audit documentation.
Related Related products and materials
Customer requirements
Leave your contact details and requirements so we can get in touch.